The foaming agent must be stirred thoroughly. Higher speed cause to a finer dispersion, what leads to a evenly distributed foam-structure. An additional thixotropig with (approx. 5 % by weight) HP-PK22, cause to a better foam up and a more homogeneous foam structure.
Technical data:
Recommended levels: |
0,5 - 4 % |
Viscosity: |
< 20 mPas (20°C), dünnflüssig
|
Density: |
0,8 g / mL (20°C) |